TPE Monprene® OM-10275,热塑性弹性体TPE,包胶热塑性弹性体TPE,包胶PP热塑性弹性体TPE,包胶PA尼龙热塑性弹性体TPE,包胶PA6热塑性弹性体TPE,包胶PA66热塑性弹性体TPE,包胶POM热塑性弹性体TPE,包胶PE热塑性弹性体TPE,包胶ABS热塑性弹性体TPE,包胶PC+ABS热塑性弹性体TPE,包胶PC热塑性弹性体TPE,包胶PS热塑性弹性体TPE,包胶ASA热塑性弹性体TPE,包胶PMMA热塑性弹性体TPE,包胶SAN热塑性弹性体TPE,包胶PBT热塑性弹性体TPE,包胶PPO热塑性弹性体TPE,包胶热塑性弹性体TPE是东莞市双帮塑胶原料有限公司常年销售的塑料,因为塑料价格行情每天都有新变化前天的报价不等于今天的报价。本公司销售的所有原料保证是原厂原包,随料可以提供生产厂商提供的物性表,SGS报告,COA原料出厂报告,REACH报告,SVHC报告,生物兼容报告,UL黄卡,提供原料注塑加工工程中可能出现的各种异常现象解决方法,塑料牌号太多,本网站没有提供的本公司也有代理,详情请咨询本公司相关业务人员0769-87795123,微信:13549213581 QQ:15397858 13549213581 肖生
医疗级TPE,TPE 75A,医疗护理用品
Monprene® OM-10275
热塑性弹性体
Teknor Apex 公司
Technical Data
产品说明
Monprene OM-10275 is designed for overmolding applications like grips and anti-skid parts for consumer/industrial products. Monprene OM-10275 is a medium hardness, medium density, opaque grade that exhibits excellent adhesion to PC, ABS, and PC/ABS.
总览
材料状态 • 已商用:当前有效
资料 1 • Technical Datasheet
搜索 UL 黄卡 • Teknor Apex 公司
• Monprene®
供货地区 • 北美洲 • 拉丁美洲 • 亚太地区
• 非洲和中东 • 欧洲
• Without Fillers • 良好的成型性能 • 中等流动性
• 光滑性 • 良好的着色性
特性 • 中等密度
• 光稳定 • 润滑
• 中等硬度
• 可粘结性 • 脱模性能良好
• 把手 • 手机 • 牙齿应用领域
• 包覆成型 • 体育用品
用途 • 电器用具 • 文具 • 牙刷柄
• 动力/其它工具 • 橡胶取代 • 粘合
• 柔软的把手 • 旋钮
RoHS 合规性 • RoHS 合规
外观 • 不透明 • 可用颜色
• 黑色 • 自然色
形式 • 粒子
加工方法 • 注射成型
物理性能 额定值单位制 测试方法
密度 / 比重 0.998g/cm³ ASTM D792
熔流率(熔体流动速率) (190°C/2.16 kg) 7.0g/10 min ASTM D1238
弹性体 额定值单位制 测试方法
拉伸应力 3 ASTM D412
横向流量 : 100%应变 3.12MPa
流量 : 100%应变 4.78MPa
横向流量 : 300%应变 5.05MPa
流量 : 300%应变 6.47MPa
抗张强度 3 ASTM D412
横向流量 : 断裂 8.20MPa
流量 : 断裂 9.88MPa
伸长率 3 ASTM D412
横向流量 : 断裂 580%
流量 : 断裂 660%
撕裂强度 3 ASTM D624
横向流量 45.9kN/m
流量 53.1kN/m
压缩永久变形 4 ASTM D395B
23°C, 22 hr 47%
70°C, 22 hr 90%
硬度 额定值单位制 测试方法
肖氏硬度 ASTM D2240
邵氏 A, 1 秒, 注塑 65
邵氏 A, 1 秒, 注塑 5 78
邵氏 A, 5 秒, 注塑 5 75
Monprene® OM-10275
热塑性弹性体
Teknor Apex 公司
补充信息 额定值单位制
Adhesion to ABS Adhesion to PC Adhesion to PC/ABS
法律声明
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
注射 额定值单位制
干燥温度 60°C
干燥时间 2.0 到 4.0hr
料筒后部温度 138 到 160°C
料筒中部温度 182 到 199°C
料筒前部温度 182 到 199°C
射嘴温度 193 到 210°C
加工(熔体)温度 177 到 199°C
模具温度 10 到 32°C
注塑压力 1.38 到 5.52MPa
背压 0.172 到 0.862MPa
螺杆转速 50 到 100rpm
垫层 3.81 到 25.4mm
注射说明
Moisture can degrade the material. Drying is suggested. This can be accomplished by placing the material in a desiccant dryer for 2 to 4 hours at 140°F (60°C).
For any overmolding process it is recommended that the process temperatures for the TPE material be set at least 50°F (10°C)higher than the melt temperature of the substrate material.
TPE Monprene® OM-10275,热塑性弹性体TPE,包胶热塑性弹性体TPE,包胶PP热塑性弹性体TPE,包胶PA尼龙热塑性弹性体TPE,包胶PA6热塑性弹性体TPE,包胶PA66热塑性弹性体TPE,包胶POM热塑性弹性体TPE,包胶PE热塑性弹性体TPE,包胶ABS热塑性弹性体TPE,包胶PC+ABS热塑性弹性体TPE,包胶PC热塑性弹性体TPE,包胶PS热塑性弹性体TPE,包胶ASA热塑性弹性体TPE,包胶PMMA热塑性弹性体TPE,包胶SAN热塑性弹性体TPE,包胶PBT热塑性弹性体TPE,包胶PPO热塑性弹性体TPE,包胶热塑性弹性体TPE是东莞市双帮塑胶原料有限公司常年销售的塑料,因为塑料价格行情每天都有新变化前天的报价不等于今天的报价。本公司销售的所有原料保证是原厂原包,随料可以提供生产厂商提供的物性表,SGS报告,COA原料出厂报告,REACH报告,SVHC报告,生物兼容报告,UL黄卡,提供原料注塑加工工程中可能出现的各种异常现象解决方法,塑料牌号太多,本网站没有提供的本公司也有代理,详情请咨询本公司相关业务人员0769-87795123,微信:13549213581 QQ:15397858 13549213581 肖生